7. Linen(hemp cloth)'s inspection method
a. Demerit mark of defects' length.

(¥°) Under width x length 1"'s defect : Demerit mark 1 point (1 point)

( ¥± ) Width x length 1.5"'s defect : Demerit mark 2 point (3 point)

( ¥² ) Width x length 5" half width's defect : Demerit mark 3 point (5 point)

( ¥³ ) Width x length over half width's defect : Demerit mark 4 point (10 point)

 
b. Material hole's defects is 4 point of demerit mark without the size.(10 point)
 
c. Flexion must be within 3% of whole width.

(44"'s case, it allowed within 1.3")

 
d. To make a standard 50yds, demerit mark must be within 13 point in every 1 ROLL.

 